Tempered glass is obtained by first cutting ordinary annealed glass to the required size, then heating it to around 700 degrees Celsius, which is close to the softening point, and finally cooling it rapidly and evenly. Generally, 5-6MM thick glass is heated at 700 degrees Celsius for about 240 seconds and then cooled for about 150 seconds. 8-10MM glass is heated at 700 degrees Celsius for about 500 seconds and then cooled for about 300 seconds. After tempering treatment, uniform compressive stress is formed on the surface of the glass, while tensile stress is formed inside, which enhances the bending and impact strength of the glass. Its strength is more than four times that of ordinary annealed glass.
The curvature of tempered glass refers to the flatness of its surface, which is usually expressed in two forms: bow-shaped and wavy. The bow-shaped curvature refers to the ratio of the maximum height difference between the raised and flat parts of the glass surface to the length of the glass, while the wavy curvature refers to the degree of undulation on the glass surface in a wavy pattern. In China, the standard for the bending degree of tempered glass is mainly stipulated by the national standard "Safety Glass for Buildings - Part 2: Tempered Glass" GB15763.2-2005. This standard indicates that the bending degree of flat tempered glass should not exceed 0.3% when bow-shaped and 0.2% when wave-shaped. These standards ensure the quality and safety of tempered glass, especially in its application in the construction field.

1.Tempered glass: Degree of tempering =2-4N/cm, surface stress α of tempered glass for glass curtain walls ≥95Mpa.
2. Semi-tempered glass: Tempering degree =2N/cm, surface stress of semi-tempered glass for glass curtain walls 24Mpa≤α≤69Mpa.
3. Super tempered glass: Tempering degree >4N/cm.
Tempered glass is obtained by first cutting ordinary annealed glass to the required size, then heating it to around 700 degrees Celsius, which is close to the softening point, and then rapidly and evenly cooling it (typically, 5-6MM thick glass is heated at 700 degrees Celsius for about 240 seconds and cooled for about 150 seconds). 8-10MM glass is heated at 700 degrees Celsius for about 500 seconds and then cooled for about 300 seconds.

After tempering treatment, uniform compressive stress is formed on the surface of the glass, while tensile stress is formed inside, which enhances the bending and impact strength of the glass. Its strength is more than four times that of ordinary annealed glass. Tempered glass that has undergone tempering treatment must not be cut, ground or subjected to any other processing or be damaged; otherwise, it will shatter into pieces due to the disruption of the uniform compressive stress balance.